Skip to main navigation Skip to search Skip to main content

Characteristics of amorphous Bi2Ti2O7thin films grown by atomic layer deposition for memory capacitor applications

  • Gyu Weon Hwang
  • , Wan Don Kim
  • , Yo Sep Min
  • , Young Jin Cho
  • , Cheol Seong Hwang
  • Seoul National University
  • Samsung

Research output: Contribution to journal › Article › peer-review

33 Scopus citations

Abstract

Bi2Ti2O7films were deposited on sputtered Ru/SiO2/Si substrates by atomic layer deposition using tris(1-methoxy-2-methyl-2-propoxy)bismuth [Bi(mmp)3], titanium tetraisopropoxide as Bi and Ti precursors, and H2O as oxidant, respectively. The wafer temperature was varied from 225 to 300°C. The growth rates decreased from 0.075nm/cycle at 225°C to 0.055nm/cycle at 300°C. The Bi concentration in the film decreased with increasing growth temperature and it could be controlled within a certain range by changing the Bi feeding at a given temperature. The as-grown Bi2Ti2O7films were amorphous but contained metallic Bi at high growth temperatures and high Bi concentrations. Bi and Ti piled-up on the film surface and the Ru interface, respectively. The electrical leakage property of the Bi2Ti2O7thin film became worse with increasing deposition temperature and Bi concentration due to the metallic Bi formation. The dielectric constant at the optimum deposition condition (225°C) was ∼40, and the leakage current level was <10-7A/cm2at 1.0MV/cm at a film thickness of ∼15nm. Reasonable conformal film thickness and cation composition over contact holes with a diameter of 0.15μm and a depth of 1.1μm were obtained.

Original languageEnglish
Pages (from-to)F20-F26
JournalJournal of the Electrochemical Society
Volume153
Issue number1
DOIs
StatePublished - 1 Jan 2006

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy

Fingerprint

Dive into the research topics of 'Characteristics of amorphous Bi2Ti2O7thin films grown by atomic layer deposition for memory capacitor applications'. Together they form a unique fingerprint.