Skip to main navigation Skip to search Skip to main content

Effect of heating rate in carbonization on mechanical properties of polyacrylonitrile based carbon fibers

  • Dawon Jang
  • , Han Ik Joh
  • , Bon Cheol Ku
  • , Seoung Ryoung Kim
  • , Yun Hyuk Bang
  • , Sungho Lee
  • Korea Institute of Science and Technology
  • University of Science and Technology UST
  • Technology Commercialization Center

Research output: Contribution to journal › Article › peer-review

2 Scopus citations

Abstract

Three types of commercially available polyacrylonitrile (PAN) fibers such as Hyosung (HS), Blue star (BS), and Jilin (JL) fibers were stabilized by continuous system and followed by carbonization at 1050 °C with heating rates of 2 and 10 °C/min in a tubular furnace. To investigate structures of resulting carbon fibers (CFs), X-ray diffraction (XRD) and Raman spectroscopy were performed. Without regarding heating rate in carbonization and types of PAN fibers, structural properties were not significantly different. However, a lower heating rate resulted in higher tensile strength with all types of PAN fibers. CFs based on HS PAN fibers showed tensile strength of ∼4.1 and ∼2.6 GPa with heating rates of 2 and 10°C/min, respectively. Tensile modulus also increased with a lower heating rate, and the values of HS CFs are ∼253 (2 °C/min) to ∼196 GPa (10 °C/min). X-ray photoelectron spectroscopy (XPS) revealed that CFs prepared with slow heating contained higher content of sp3 even though there was no significant different in carbon content. These suggest that chemical structure play an important role in mechanical properties of CFs.

Original languageEnglish
Pages (from-to)196-202
Number of pages7
JournalPolymer (Korea)
Volume41
Issue number2
DOIs
StatePublished - Mar 2017

Keywords

  • Carbon fiber
  • Carbonization
  • Polyacrylonitrile
  • Stabilization
  • Tensile properties

Fingerprint

Dive into the research topics of 'Effect of heating rate in carbonization on mechanical properties of polyacrylonitrile based carbon fibers'. Together they form a unique fingerprint.

Cite this