Oxyapatite phosphors with the composition Sr2La8-x(SiO4)6O2:xGd3+ were successfully prepared through a simple sol–gel synthesis method. Powder X-ray diffraction patterns confirmed the formation of a hexagonal oxyapatite structure with good crystallinity across all compositions. Scanning electron microscopy further showed that the phosphor powders are composed of fine particles, uniformly distributed within larger agglomerated clusters. Photoluminescence measurements demonstrate that the intensity of the characteristic emission band centered at ∼314 nm increases systematically with increasing Gd³⁺ concentration under 228 nm excitation. This emission is attributed to the 6P7/2 → 8S7/2 electronic transition of Gd3+. This strong emission response, together with the structural stability of the host, indicates that Sr2La8-x(SiO4)6O2:xGd3+ material demonstrates efficient UV-B emission, underscoring the material’s potentiality for use in UV emitting phosphor applications. The room-temperature electron paramagnetic resonance (EPR) spectrum exhibits overlapping dominant lines with g values of ∼1.97 and ∼1.95. Other EPR lines are seen at g ∼ 5.7, 2.8, 2.2 and 1.7. Low field lines in the spectrum arise from distortions in the environment of the substitutional Gd3+ ion.
| Original language | English |
|---|---|
| Article number | 145847 |
| Journal | Journal of Molecular Structure |
| Volume | 1365 |
| DOIs | |
| State | Published - 15 Jul 2026 |
Keywords
- EPR
- Gd3+ions
- Photoluminescence
- Sol-Gel
- SrLa(SiO)O
Fingerprint
Dive into the research topics of 'Efficient UVB photoluminescence in sol–gel-derived Gd3+-incorporated Sr2La8(SiO4)6O2 oxyapatite'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver