Abstract
YAG phosphor powders doped/codoped with Er3+/(Er3+ + Yb3+) have been synthesised by using the solution combustion method. The effect of direct pumping into the 4I11/2 level under 980 nm excitation of doped/codoped Er3+/Yb3+-Er 3+ in Y3Al5O12 (YAG) phosphor responsible for an infrared (IR) emission peaking at ∼1.53 μm corresponding to the 4I13/2→4I 15/2 transition has been studied. YAG exhibits three thermally-stimulated luminescence (TSL) peaks at around 140°C, 210°C and 445°C. Electron spin resonance (ESR) studies were carried out to identify the centres responsible for the TSL peaks. The room temperature ESR spectrum of irradiated phosphor appears to be a superposition of two distinct centres. One of the centres (centre I) with principal g-value 2.0176 is identified as O - ion, while centre II with an isotropic g-factor 2.0020 is assigned to an F+ centre (singly ionised oxygen vacancy). An additional defect centre is observed during thermal-annealing experiments and this centre (assigned to F+ centre) seems to originate from an F-centre (oxygen vacancy with two electrons) and these two centres appear to correlate with the observed high-temperature TSL peak in YAG phosphor.
| Original language | English |
|---|---|
| Pages (from-to) | 1123-1130 |
| Number of pages | 8 |
| Journal | Applied Physics A: Materials Science and Processing |
| Volume | 100 |
| Issue number | 4 |
| DOIs | |
| State | Published - Sep 2010 |
Fingerprint
Dive into the research topics of 'Infrared emission and defect centres in Er and Yb codoped Y 3Al5O12 phosphors'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver