Abstract
Manganese-activated strontium hexa-aluminate (SrAl12O19) phosphor has been prepared at low temperature (500 °C) and in a very short time (<5 min) by urea combustion route. Powder X-ray diffraction pattern showed the presence of hexagonal SrAl12O19 phase. Scanning electron microscopy (SEM) indicated the presence of several particles with sizes of 200 nm. The luminescence of Mn2+ activated SrAl12O19 exhibits a strong green emission peak around 515 nm from the synthesized phosphor particles under excitation (451 nm). The luminescence is assigned to a transition from the upper 4T1→6A1 ground state of Mn2+ ions. EPR investigations also indicated the presence of Mn2+ ions in the prepared material. From the observed EPR spectrum, the spin-Hamiltonian parameters have been evaluated. The magnitude of the hyperfine splitting (A) constant indicates that there exists a moderately covalent bonding between Mn2+ ions and the surrounding ligands. The variation of zero-field splitting parameter (D) with temperature is measured and discussed. The mechanism involved in the generation of a green emission has been explained in detail.
| Original language | English |
|---|---|
| Pages (from-to) | 120-125 |
| Number of pages | 6 |
| Journal | Physica B: Condensed Matter |
| Volume | 403 |
| Issue number | 1 |
| DOIs | |
| State | Published - 1 Jan 2008 |
Keywords
- Combustion
- EPR
- Mn ions
- Phosphors
- Photoluminescence
Fingerprint
Dive into the research topics of 'Luminescence and EPR studies of Mn-activated SrAl12O19 phosphor prepared by facile combustion approach'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver