Pyridine-Catalyzed Atomic Layer Deposition of SiO2from Hexachlorodisilane and Water: An in Situ Mechanistic Study

  • Jieun Hyun
  • , Hyeongjin Kim
  • , Bonggeun Shong
  • , Yo Sep Min
  • Konkuk University
  • Hongik University

Research output: Contribution to journal › Article › peer-review

8 Scopus citations

Abstract

Pyridine-catalyzed atomic layer deposition (ALD) of SiO2from hexachlorodisilane and water was studied by in situ analyses using Fourier-transform infrared spectrometry and a quartz crystal microbalance. Although it has been observed that ALD SiO2can grow even when only one half-reaction is catalyzed, typical self-limiting growth of SiO2by catalytic ALD has been achieved when both half-reactions are catalyzed by pyridine. The in situ analyses revealed that the unexpected growth of SiO2, when only one half-reaction was catalyzed, was caused by the presence of residual pyridine that had not yet desorbed from the previous half-reaction. The retardation of catalyst desorption was more prominent on the OH-terminated SiO2surface than on the Cl-terminated surface, which is related to the significantly higher desorption energy of pyridine species on the hydroxyl surface calculated using density functional theory.

Original languageEnglish
Pages (from-to)4100-4108
Number of pages9
JournalChemistry of Materials
Volume35
Issue number10
DOIs
StatePublished - 23 May 2023