Abstract
Y2SiO5 (YSO) phosphors doped with holmium ions were prepared by the well-established sol–gel method. The structural and functional groups were studied by X-ray diffraction (XRD) and Fourier-transformed infrared (FTIR) spectroscopy, respectively. The observed XRD peaks were matched to the X1 and X2 phase of YSO and the average crystalline size is found to be 26.5 nm. The band gap was calculated using Kubelka–Munk analysis of the diffuse reflectance data. Photoluminescence tests were carried out on the prepared phosphors. At an excitation wavelength of 447 nm, two sharp and closely spaced peaks are observed in the green region around 538 nm and 551 nm. The concentration quenching is observed beyond 0.03 mol Ho3+ ions in YSO and the energy transfer mechanisms are discussed in detail. Dexter’s analysis shows that the interaction between Ho3+ ions is dipole–dipole. The Judd–Ofelt intensity parameters and radiative properties of certain emission transitions of Ho3+ ions were also investigated for an optimized phosphor (Y2SiO5:0.03Ho3+) sample. The estimated J–O parameters (Ωλ (λ = 2, 4 & 6)), are Ω2 = 0.77 × 10–20 cm2, Ω4 = 0.40 × 10–20 cm2 and Ω6 = 2.12 × 10–20 cm2. The magnitude of Ω2 is smaller for YSO than that of other hosts indicating a less asymmetric environment around the Ho–O bond. Branching ratio and stimulated emission for the 5F4 + 5S2 → 5I8 transition are 87.8% and 2.61 × 10–21 cm2, respectively, for Y2SiO5:0.03Ho3+ phosphor. Furthermore, colorimetric analysis shows that the optimized Y2SiO5:0.03Ho3+ phosphor has the highest color purity. Our results confirm that these phosphors can be proposed for utilization as green components in solid-state lighting applications.
| Original language | English |
|---|---|
| Article number | 2304 |
| Journal | Journal of Materials Science: Materials in Electronics |
| Volume | 34 |
| Issue number | 36 |
| DOIs | |
| State | Published - Dec 2023 |
Fingerprint
Dive into the research topics of 'Radiative properties of green-emitting Ho3+ doped Y2SiO5 system: exploring the potential use as a phosphor'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver