Abstract
Porous wollastonite (CaSiO3) powders were fabricated by a polymer solution technique. Silica sol and calcium nitrate were dissolved in de-ionized water without any precipitation, and polyvinyl alcohol (PVA) was mixed as a polymer carrier. An explosive exothermic reaction during the calcination process resulted in a porous powder structure. The crystalline development and specific surface areas of the calcined powders were dependant on the polymer content and type of silica sol. The porous powders were crystallized to β-CaSiO3 at a lower temperature of about 900°C than that of other synthesis methods, and the calcined powders were ball-milled to fine particles and densified at 1200°C with an uniform grain size of α phase.
| Original language | English |
|---|---|
| Pages (from-to) | 298-301 |
| Number of pages | 4 |
| Journal | Journal of Ceramic Processing Research |
| Volume | 6 |
| Issue number | 4 |
| State | Published - 2005 |
Keywords
- Ball milling
- Polyvinyl alcohol
- Porous particles
- Powder technology
- Sintering
- Wollastonite
Fingerprint
Dive into the research topics of 'Synthesis and sintering behavior of wollastonite fabricated by a polymer solution technique'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver